University of Leicester
Browse

Seeding of single-crystal superalloys — Role of constitutional undercooling and primary dendrite orientation on stray-grain nucleation and growth

Download (1.87 MB)
journal contribution
posted on 2009-12-08, 16:16 authored by N. D'Souza, P. A. Jennings, X. L. Yang, Hongbiao Dong, P. D. Lee, M. McLean
An experimental study, together with a two-dimensional numerical simulation of solute segregation, was conducted to investigate (1) the mechanism for stray-grain nucleation following seed melt-back and initial withdrawal and (2) the role of the primary dendrite disposition of the seed crystal in relation to the mold wall during growth. It is proposed that the factors contributing to stray-grain nucleation during initial withdrawal are (1) the magnitude of local, solute-adjusted undercooling and (2) the rapidly changing curvature of the solidification front close to the mold walls during the initial solidification transient. Based upon the calculated local undercooling and experimentally observed stray-grain morphologies, it was concluded that stray grains nucleate near the mold wall around the seed perimeter and behind the columnar dendrites that advance into the bulk liquid ahead of the melt-back zone. These grains then compete during growth with the dendrites originating from the seed. Therefore, the morphological constraints arising from the inclination of the primary dendrites from the seed crystal with respect to the mold wall (converging/diverging/axial 〈001〉) determines the probability of the stray-grain nuclei developing into equiaxed/columnar grains following competitive growth.

History

Citation

Metallurgical and Materials Transactions B, 2005, 36 (5), pp. 657-666

Version

  • VoR (Version of Record)

Published in

Metallurgical and Materials Transactions B

Publisher

Springer Verlag on behalf of ASM International

issn

1073-5615

eissn

1543-1916

Copyright date

2005

Available date

2009-12-08

Publisher version

http://link.springer.com/article/10.1007/s11663-005-0056-6

Notes

This paper was published in Metallurgical and Materials Transactions B, 2005, Volume 36, Issue 5, pp. 657-666 and is made available as an electronic reprint with the permission of ASM International. One print or electronic copy may be made for personal use only. Systematic or multiple reproduction, distribution to multiple locations via electronic or other means, duplications of any material in this paper for a fee or for commercial purposes, or modification of the content of this paper are prohibited.

Language

en

Usage metrics

    University of Leicester Publications

    Categories

    No categories selected

    Keywords

    Exports

    RefWorks
    BibTeX
    Ref. manager
    Endnote
    DataCite
    NLM
    DC