Transition from internal to surface crack initiation of a single-crystal superalloy in the very-high-cycle fatigue regime at 1100 °C

Download (13.4 MB)
journal contribution
posted on 2021-07-01, 14:12 authored by Z Zhao, Q Li, F Zhang, W Xu, B Chen
Transition from internal to surface crack initiation is controlled by oxidation assisted fatigue-crack process in the very-high-cycle fatigue regime. Between 760 and 1000 °C, single crack initiation site is associated with internal casting defect, followed by a crystallographic Stage I propagation. By contrast, multiple surface crack initiation sites appear at 1100 °C, as the consequence of internal oxide penetration. The fatal crack follows a Mode I propagation and oxygen can diffuse into the material along the crack path. γ′-phase depletion appears surrounding the oxidised and cracked regions, while localised rafting can occur close to the crack tip.

History

Citation

International Journal of Fatigue, Volume 150, September 2021, 106343

Author affiliation

School of Engineering

Version

  • AM (Accepted Manuscript)

Published in

International Journal of Fatigue

Volume

150

Pagination

106343

Publisher

Elsevier BV

issn

0142-1123

Acceptance date

2021-05-19

Copyright date

2021

Available date

2022-05-24

Language

en

Usage metrics

    University of Leicester Publications

    Categories

    No categories selected

    Exports

    RefWorks
    BibTeX
    Ref. manager
    Endnote
    DataCite
    NLM
    DC